Corrosion Study and Surface Analysis of the Passivation Film on Surface-Deformed AISI 304 Stainless Steel

Temitope Olumide Olugbade (Lead / Corresponding author), Babatunde Olamide Omiyale

Research output: Contribution to journalArticlepeer-review

4 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Corrosion Study and Surface Analysis of the Passivation Film on Surface-Deformed AISI 304 Stainless Steel'. Together they form a unique fingerprint.

Engineering

Material Science