Positron Annihilation Spectroscopy Studies of Energy Materials

  • Aryaveer Singh

Student thesis: Doctoral Thesis › Doctor of Philosophy

Abstract

This thesis uses positron annihilation lifetime spectroscopy (PALS), both variable energy (VE) PALS that can profile from the surface down to depths typically of 1– 2 µm, and conventional PALS using unmoderated 22Na positrons with varying energies that implant to varying depths down to ~100– 300 µm below the surface. The methods have been applied to gain insight on vacancy-related point defects in materials used in energy technologies, specifically Zircaloy-4 and tungsten which have application in nuclear fission and fusion reactors, respectively, and metal halide perovskites (MHP) materials, ABX3, that are under development as absorber layers for solar cells.

Zircaloy-4 subjected to self-ion implantation with and without the presence of hydrogen was studied. The aim was to gain insight on the interactions between vacancy defects and hydrogen as this is thought to contribute to corrosion in reactor environments. It was found that vacancy defect concentrations in the top ~1 µm of the as-received samples exceeded the positron saturation trapping limit, which made it difficult to resolve meaningful differences when the samples were subjected to Zr-ion implantation with and without the presence of hydrogen.

Tungsten is the primary candidate as the plasma facing cladding in fusion reactors, in which the materials are subjected to 14 MeV neutron irradiation. Positron lifetime measurements provide a means of detecting and quantifying the monovacancy defect, the initial defect generated during particle irradiation. Despite the fundamental importance of tungsten in this role there is currently still some uncertainty in the positron parameters for pure tungsten and the monovacancy defect. In this work VE-PALS and conventional PALS measurements on high-purity annealed single crystal tungsten established that the perfect lattice, bulk, positron lifetime lies within the range 103 ps and 108 ps and a value of 105(3) ps is reported. Similar measurements on a pair of similar crystals subjected to 4.5 MeV electron irradiation clearly resolved a component due to positron trapping into vacancy defects with lifetime in the range 176 ps to 182 ps. However, the limitations of the spectrum deconvolution process prevented a more accurate and precise value for the monovacancy lifetime from being obtained.

In this work VE-PALS measurements were performed on the perovskite materials MAPbI3, FAPbI3, MAPbBr3, FAPbBr3, CsPbBr3, MAPbCl3 and CsPbCl3 samples including single crystals and thin films, and on (CsxFA1−x)PbI3, (Cs0.1FA0.9)PbI2.9Br0.1, (Cs0.05FA0.85MA0.10)PbI3 and CsPbCl1−yBry films. Conventional PALS measurements were made on MAPbBr3 and CsPbBr3 single crystal pairs. Positron lifetime components attributed to positron trapping to B-site  V 2− Pb defects have been identified for each APbX3 material. A positron lifetime component in the approximate range ~420 ps to 480 ps was observed from certain samples of MAPbI3, FAPbI3, MAPbBr3, FAPbBr3, CsPbBr3 and (Cs0.1FA0.9)PbI2.9Br0.1 and is attributed to positron trapping at A-site vacancy, V 1−A , defects, in agreement with two-component density functional theory calculations. The VE-PALS spectra measured from almost all MHP samples studied exhibited positron trapping to concentrations of vacancy defects close to or above the saturation trapping threshold, which can be estimated to be ~ 7 ×1016 cm−3. The conventional PALS measurements, which are probing primarily deeper than the 1– 2 µm near surface region, observed dominant component due to positron annihilations from the perfect lattice state. This enabled experimental values for the perfect lattice, bulk, positron state lifetimes, as well as vacancy defect concentrations, to be obtained.
Date of Award2026
Original languageEnglish
Awarding Institution
  • University of Dundee
SupervisorDavid Keeble (Supervisor)

Keywords

  • Positron annihilation Spectroscopy, Point defects, Energy materials, Zircaloy-4, Tungsten, Metal halide perovskites

Cite this

'